Study of high-temperature processes at interphase boundary of chromium (titanium) and alumina /
The experiments were carried out at 1600°C for 4-hour periods under a pressure of 1.2 bar Ar (melting of Ni-Cr, Ni-CrTi alloys and high-temperature exposure of vacuum-deposited layers), and at 1900°C or 1720°C for 25-minute periods under a pressure of 1.2 bar Ar (melting of pure chromium or titanium...
Hlavní autor: |
Maca, Karel, 1964-
(
Autor )
|
---|---|
Další autoři: |
Cihlář, Jaroslav, 1946-
(
Autor )
|
Typ dokumentu: | Článek |
Jazyk: |
angličtina |
ISSN: | 0862-5468 |
Zdroj: | Ceramics - Silikáty: Ročník 41, číslo 1, strana 13-20. |