Endocrown em CAD-CAM : an?lise in vitro da carga m?xima de fratura e do modo de falha

Autor: Slomp, Cilea
Jazyk: portugalština
Rok vydání: 2015
Předmět:
Zdroj: Biblioteca Digital de Teses e Dissertações da PUC_RSPontifícia Universidade Católica do Rio Grande do SulPUC_RS.
Druh dokumentu: masterThesis
Popis: Submitted by Setor de Tratamento da Informa??o - BC/PUCRS (tede2@pucrs.br) on 2015-07-30T17:24:02Z No. of bitstreams: 1 472793 - Texto Completo.pdf: 1578702 bytes, checksum: 6981999ba7f8dee786191519497e2438 (MD5)
Made available in DSpace on 2015-07-30T17:24:02Z (GMT). No. of bitstreams: 1 472793 - Texto Completo.pdf: 1578702 bytes, checksum: 6981999ba7f8dee786191519497e2438 (MD5) Previous issue date: 2015-03-06
Coordena??o de Aperfei?oamento de Pessoal de N?vel Superior - CAPES
Objectives : To evaluate the maximum fracture load and the failure pattern of endodontically treated molars restored with endocrown by CAD-CAM system. Methods : Thirty healthy extracted molars were randomly assigned into 3 groups (n=10). After endodontic treatment, teeth were restored with endocrowns by CEREC/InLab (Sirona) system with three different materials: e.max CAD (Ivoclar Vivadent), Vita Mark II (VITA) or Lava Ultimate (3M ESPE). The specimens were subjected to the fractured resistance testing after 1,000,000 cyclic fatigue loading at 100N. Subsequently, they were tested in a universal testing machine with a crosshead speed of 1mm/min with compressive force to the long axis of the tooth. Results : According to a 2-way analysis of variance, the means of fracture resistence were (means followed by the same letter show no significant difference to ANOVA and Tukey) (p
Objetivos : avaliar a carga m?xima de fratura e o padr?o de falha de restaura??es endocrown realizadas com sistema CAD-CAM cimentadas sobre molares tratados endodonticamente. Materiais e m?todos : trinta dentes molares h?gidos extra?dos foram distribu?dos aleatoriamente em 3 grupos (n=10). Ap?s serem endodonticamente tratados, foram restaurados com endocrowns realizadas atrav?s do sistema CEREC/InLab (Sirona) com tr?s diferentes materiais: e.max CAD (Ivoclar Vivadent), Vita Mark II (VITA) ou Lava Ultimate (3M ESPE). Ap?s, foram submetidos ? fadiga mec?nica com aplica??o de carga vertical de 100N, totalizando 1.000.000 de ciclos. Posteriormente, foi testada a carga m?xima de fratura com for?a compressiva ao longo eixo do dente sob velocidade de 1mm/min. Resultados : Os resultados obtidos ap?s o ensaio de carregamento m?ximo de fratura foram (m?dias seguidas de mesma letra n?o apresentam diferen?a estat?stica para ANOVA e Tukey) (p
Databáze: Networked Digital Library of Theses & Dissertations