Three-dimensional microstructural mapping of poisoning phases in the Neodymium Nickelate solid oxide fuel cell cathode
Autor: | Harris, William M., Lombardo, Jeffrey J., DeGostin, Matthew B., Nelson, George J., Luebbe, Henning, Schuler, J. Andreas, Van herle, Jan, Andrews, Joy C., Liu, Yijin, Pianetta, Piero, Karen Chen, Yu-Chen, Wang, Jun, Chiu, Wilson K.S. |
---|---|
Zdroj: | In Solid State Ionics 15 April 2013 237:16-21 |