Effect of Dentin Desensitizers and Nd:YAG Laser Pre-Treatment on Microshear Bond Strength of Adhesive Resin Cement to Dentin
Autor: | Fatih Sarı, Onur Şahin, Ali Kemal Özdemir |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2019 |
Předmět: | |
Zdroj: | Cumhuriyet Dental Journal, Vol 22, Iss 2, Pp 156-166 (2019) |
Druh dokumentu: | article |
ISSN: | 1302-5805 2146-2852 |
DOI: | 10.7126/cumudj.537953 |
Popis: | Objectives: The aim of this study was to evaluate how microshear bond strength of different adhesive resin cements are affected by dentin desensitizers application and preparation depth. Materials and Methods: One hundred and forty-four maxillary incisors were randomly divided into two groups according to dentin preparation depth (0.8 and 1 mm) and each group subdivided into four dentin desensitizers, Nd:YAG (Neodymium-doped Yttrium aluminum Garnet) laser and control groups. The dentin desensitizers used were Gluma [Glutaraldehyde/ Hydroxyethyl methacrylate (HEMA)], BisBlock (Oxalate) Vivasens-Potassium Fluoride (KF) and Admira Protect (Ormocer/HEMA), respectively. Three dual cure resin based luting cement (RelyX ARC; Variolink II and Maxcem Elite) were used to create a 0,7 mm diameter and 1 mm height cylindirical shape buid-up in tygon tubes (n=10). Micro-shear bond strength (µSBS) test was performed at a crosshead of speed of 0.5 mm/min using a Universal testing device. Then tooth surface was investigated by steromicroscope and scanning electron microscopy (SEM). Data were analyzed using Kruskal-Wallis, Mann-Whitney U and Chi-Square (X2) tests. (p = 0.05)Results: There was no statistically difference between the groups at 0.8 mm preparation depth. At 1 mm preparation dept RelyX ARC + Gluma groups’ mean bond strength value (23.96 ± 6.66 MPa) was found statistically lower according to the other groups (p0.05). |
Databáze: | Directory of Open Access Journals |
Externí odkaz: |