Early and late hydration of supersulphated cements of blast furnace slag with fluorgypsum
Autor: | M. E. Bazaldúa-Medellín, A. F. Fuentes, A. Gorokhovsky, J. I. Escalante-García |
---|---|
Jazyk: | English<br />Spanish; Castilian |
Rok vydání: | 2015 |
Předmět: | |
Zdroj: | Materiales de Construccion, Vol 65, Iss 317, Pp e043-e043 (2015) |
Druh dokumentu: | article |
ISSN: | 0465-2746 1988-3226 |
DOI: | 10.3989/mc.2015.06013 |
Popis: | The hydration, strength development and composition of hydration products of supersulphated cements were characterized from the first 48 hours up to 360 days. Two compositions of 80% Blast furnace slag, 10–15% Fluorgypsum and 10–5% Portland cement were cured in dry and wet conditions. The main hydration products were ettringite and C-S-H since the first hours and up to 360 days as evidenced by X-ray diffraction, thermal analysis and electron microscopy. The strength was favored by higher fluorgypsum contents and lower Portland cement contents. These cements generated heats of hydration of 40–57 KJ/Kg after 28 hours, which are lower than portland cement. |
Databáze: | Directory of Open Access Journals |