Reduction of hazardous incinerated bio-medical waste ash and its environmental strain by utilizing in green concrete

Autor: A. Suresh Kumar, M. Muthukannan, R. Kanniga Devi, K. Arunkumar, A. Chithambar Ganesh
Jazyk: angličtina
Rok vydání: 2021
Předmět:
Zdroj: Water Science and Technology, Vol 84, Iss 10-11, Pp 2780-2792 (2021)
Druh dokumentu: article
ISSN: 0273-1223
1996-9732
DOI: 10.2166/wst.2021.239
Popis: Incinerated Bio-Medical Waste Ash (IBWA) is toxic waste material with broad potential (cancer, genetic risk, premature death, permanent disease) to inflict severe health damage for the atmosphere and humans. This waste is disposed of as landfill, which contaminates the underground water and environment. The effective way of disposal of IBWA is by utilizing it as a building material, which can reduce the hazardous toxic materials. The use of Geopolymer Concrete (GPC) combined with IBWA as a substitute for Ground Granulated Blast Furnace Slag (GGBS) has been researched for its ability to create a new type of Green Concrete. The physical and chemical properties were observed for the raw materials. IBWA was used at 0, 5, 10, 15, 20, 25, 30, 35, 40, 45 and 50% replacement by weight for GGBS. Mixing proportions were 1:2.21:3.48 respectively for GGBS, Manufacturing Sand (M-sand), and coarse aggregate. Fresh properties and mechanical properties were examined for all specimens. The findings show an increase in the setting time and flow of concrete and a decrease in density with improved utilization of IBWA. On the other hand, IBWA replacement for GGBS enhanced the mechanical properties. These results revealed that IBWA could be partially replaced as source material for Geopolymer Concrete. This research may contribute to the reduction of dangerous IBWA as a building material. HIGHLIGHTS Focus on the effective disposal of hazardous Incinerated Bio-Medical Waste Ash (IBWA).; Focus on changes in characteristics of geopolymer concrete after incorporating IBWA.; Geopolymer concrete with IBWA has excellent performance over flowability.; Compressive strength reaches over 43 MPa after 28 days of incorporating IBWA.;
Databáze: Directory of Open Access Journals