Biomechanical Assessment of Endodontically Treated Molars Restored by Endocrowns Made from Different CAD/CAM Materials
Autor: | Mhd Ayham Darwich, Abeer Aljareh, Nabil Alhouri, Szabolcs Szávai, Hasan Mhd Nazha, Fabian Duvigneau, Daniel Juhre |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2023 |
Předmět: |
dental crowns
finite element analysis CAD-CAM lithium disilicate ceramics zirconium oxide Technology Electrical engineering. Electronics. Nuclear engineering TK1-9971 Engineering (General). Civil engineering (General) TA1-2040 Microscopy QH201-278.5 Descriptive and experimental mechanics QC120-168.85 |
Zdroj: | Materials, Vol 16, Iss 2, p 764 (2023) |
Druh dokumentu: | article |
ISSN: | 1996-1944 |
DOI: | 10.3390/ma16020764 |
Popis: | The aim of this study was to evaluate the deflection and stress distribution in endodontically treated molars restored by endocrowns from different materials available for the computer-aided design/computer-aided manufacturing (CAD/CAM) technique using three-dimensional finite element analysis. The models represented extensively damaged molars restored by endocrowns from the following materials: translucent zirconia; zirconia-reinforced glass ceramic; lithium disilicate glass ceramic; polymer-infiltrated ceramic network (PICN) and resin nanoceramic. Axial and oblique loadings were applied and the resulting stress distribution and deflection were analyzed. The Mohr–Coulomb (MC) ratio was also calculated in all models. The translucent zirconia endocrown showed the highest stress concentration within it and the least stress in dental structures. The resin nanoceramic model was associated with the greatest stress concentration in dental tissues, followed by the PICN model. Stress was also concentrated in the distal region of the cement layer. The MC ratio in the cement was higher than 1 in the resin nanoceramic model. Oblique loading caused higher stresses in all components and greater displacement than axial loading, whatever the material of the endocrown was. The translucent zirconia model recorded deflections of enamel and dentin (38.4 µm and 35.7 µm, respectively), while resin nanoceramic showed the highest stress concentration and displacement in the tooth–endocrown complex. |