Popis: |
Based on the operational measurement, of which content was to determine ladle thermal profile, there were analysed causes of possible damage of lining in steel ladles by steel breakout through the ladle shell. There exists connection between thermal state of ladle lining during the operation and its lifetime. There were reached to the conclusion that the cause of failure in the lining of ladle is except for high temperature of bath, also wide interval of temperature change during the tap operation, in consequence with possible insufficient pre-heating of ladle, discontinuous operation of aggregate and damage of insulating lining layer, respectively deformation of ladles shell. |
Databáze: |
Directory of Open Access Journals |
Externí odkaz: |
|