Autor: |
R.M. Ribeiro, L.F. Lemus, D.S. dos Santos |
Jazyk: |
angličtina |
Rok vydání: |
2013 |
Předmět: |
|
Zdroj: |
Materials Research, Vol 16, Iss 3, Pp 679-682 (2013) |
Druh dokumentu: |
article |
ISSN: |
1516-1439 |
Popis: |
The hydrogen absorption and desorption of Ti53Zr27Ni20 icosahedral quasicrystal (ICQ) and Ti50Ni50 shape memory alloy (SMA) melt-spun ribbons was studied. Samples were exposed to hydrogen gas at 623 K and 4 MPa for 1000 minutes. The total capacity of hydrogen obtained for Ti53Zr27Ni20 and Ti50Ni50 was 3.2 and 2.4 wt. % respectively. The Thermal Desorption Spectrometry (TDS) of the hydrogenated alloys shows that both alloys start to desorb hydrogen around 750 K. X-ray diffraction (XRD) patterns, performed after hydrogenation, indicate a complete amorphization of the Ti53Zr27Ni20 i-phase alloy, while the Ti50Ni50 alloy remained crystalline after hydride formation. |
Databáze: |
Directory of Open Access Journals |
Externí odkaz: |
|