Autor: |
Huan Li, Weifeng Qian, Zhen Zhang, Shuang Wang, Yongnan Chen, Fengying Zhang, Zhimin Hou, Guangrui Gao, Qinyang Zhao, Haifei Zhan |
Jazyk: |
angličtina |
Rok vydání: |
2024 |
Předmět: |
|
Zdroj: |
Materials & Design, Vol 239, Iss , Pp 112741- (2024) |
Druh dokumentu: |
article |
ISSN: |
0264-1275 |
DOI: |
10.1016/j.matdes.2024.112741 |
Popis: |
In this work, the trade-off between transformation toughening of ZrO2/TiO2 ceramic coatings and low temperature (293.15 K∼203.15 K) was achieved by adjusting the grain size of t-ZrO2 (dt-ZrO2). A negative correlation between dt-ZrO2 and phase transition temperature (Ms) was also established based on strain energy and chemical free energy in ZrO2/TiO2 ceramic coatings. Interestingly, t-ZrO2 grains lost toughening effects when the dt-ZrO2 reaches the critical size (20 nm) even under cooling and stress. This is attributed to the number of dislocations per unit volume increases 1.5 times with the dt-ZrO2 decreases from 40 nm to 20 nm, which aggravates the lattice distortion and dislocation tangle and leads to the fracture toughness increases by 32.5% at 203.15 K. Therefore, the interfacial cohesion of the semi-coherent interface between (011) t-ZrO2 and (110) TiO2 was enhanced and t-ZrO2 was completely stabilized when dt-ZrO2 reaches critical size. This work elucidates the effect of size effect on Ms and provides a reference for transformation toughening of ceramic coatings at cryogenic temperature. |
Databáze: |
Directory of Open Access Journals |
Externí odkaz: |
|