Popis: |
Background: Newer dentin bonding agents were developed to improve the quality of composite restoration and to reduce time consumption in its application. The aim of the present study was to evaluate tensile bond strength of 6th, 7th and 8th generation bonding agents by in vitro method. Materials and Methods: Selected 60 permanent teeth were assigned into 20 in each group (Group I: 6th generation bonding agent-Adper SE plus 3M ESPE, Group II: 7th generation bonding agent-G-Bond GC Corp Japan and Group III: 8th generation dentin adhesives-FuturaBond, DC, Voco, Germany). With high-speed diamond disc, coronal dentin was exposed, and selected dentin bonding agents were applied, followed by composite restoration. All samples were saved in saline for 24 h and tensile bond strength testing was done using a universal testing machine. The obtained data were tabulated and statistically analyzed using ANOVA test. Results: The tensile bond strength readings for 6th generation bonding agent was 32.2465, for 7th generation was 31.6734, and for 8th-generation dentine bonding agent was 34.74431. The highest tensile bond strength was seen in 8th generation bonding agent compared to 6th and 7th generation bonding agents. Conclusion: From the present study it can be conclude that 8th generation dentine adhesive (Futura DC, Voco, Germany) resulted in highest tensile bond strength compared to 6th (Adper SE plus, 3M ESPE) and 7th generation (G-Bond) dentin bonding agents. |