The effect of a new formaldehyde-free binder on the dissolution rate of glass wool fibre in physiological saline solution
Autor: | Nassreen Olang, Russell M. Potter |
---|---|
Rok vydání: | 2013 |
Předmět: |
Materials science
Surface Properties Health Toxicology and Mutagenesis Carbohydrates Carboxylic Acids Glass wool Sodium Chloride engineering.material Toxicology Biosolubility Fibre Coating Formaldehyde medicine Particle Size Solubility Composite material Dissolution Binder Research Wool Biopersistence General Medicine Hydrogen-Ion Concentration Kinetics Ashing engineering Glass Particle size Swelling medicine.symptom |
Zdroj: | Particle and Fibre Toxicology |
ISSN: | 1743-8977 |
DOI: | 10.1186/1743-8977-10-13 |
Popis: | The in-vitro dissolution rate of fibres is a good predictor of the in-vivo behavior and potential health effects of inhaled fibres. This study examines the effect of a new formaldehyde-free carbohydrate-polycarboxylic acid binder on the in-vitro dissolution rate of biosoluble glass fibres. Dissolution rate measurements in pH 7.4 physiological saline solution show that the presence of the binder on wool insulation glass fibres has no effect on their dissolution. There is no measurable difference between the dissolution rates of continuous draw fibres before and after binder was applied by dipping. Nor is there a measurable difference between the dissolution rates of a production glass wool sample with binder and that same sample after removal of the binder by low-temperature ashing. Morphological examination shows that swelling of the binder in the solution is at least partially responsible for the development of open channels around the glass-binder interface early in the dissolution. These channels allow fluid to reach the entire glass surface under the binder coating. There is no evidence of any delay in the dissolution rate as a result of the binder coating. |
Databáze: | OpenAIRE |
Externí odkaz: |