The effect of crack path on tearing resistance of a narrow-gap Alloy 52 dissimilar metal weld
Autor: | Matias Ahonen, Teemu Sarikka, Hannu Hänninen, Sebastian Lindqvist |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2018 |
Předmět: |
Tearing resistance
Materials science Alloy 02 engineering and technology Welding engineering.material law.invention Strength mismatch 0203 mechanical engineering law Tearing mental disorders General Materials Science Composite material ta216 Fusion Dissimilar metal weld Crack path Plane (geometry) Mechanical Engineering technology industry and agriculture Fracture mechanics respiratory system 021001 nanoscience & nanotechnology Nuclear power plant 020303 mechanical engineering & transports Mechanics of Materials Path (graph theory) engineering Fracture (geology) 0210 nano-technology |
Zdroj: | Lindqvist, S, Sarikka, T, Ahonen, M & Hänninen, H 2018, ' The effect of crack path on tearing resistance of a narrow-gap Alloy 52 dissimilar metal weld ', Engineering Fracture Mechanics, vol. 201, pp. 130-143 . https://doi.org/10.1016/j.engfracmech.2018.05.043 |
ISSN: | 0013-7944 |
DOI: | 10.1016/j.engfracmech.2018.05.043 |
Popis: | Fracture mechanical testing of welds with strength mismatch can lead to deviation of the crack path from the initial crack growth plane. Current fracture mechanics standards do not give guidance for analyses of the effect of crack path on the tearing resistance. In this study, the effect of crack path on tearing resistance was investigated by fracture mechanical testing and crack path analyses of a narrow-gap Alloy 52 dissimilar metal weld. The results show that tearing resistance of HAZ cracks deviating towards the same zone close to the fusion boundary is larger for cracks initially further from the fusion boundary. The results were obtained for a specific dissimilar metal weld, but the results can also be used to interpret the effect of crack path on tearing resistance in other type of welds. |