Evaluation of hardness and wear of surface treated zirconia on enamel wear. An in-vitro study
Autor: | Mona Elagroudy, Hesham Katamish, Mostafa Aboushahba |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2018 |
Předmět: |
Materials science
medicine.medical_treatment 0206 medical engineering Y-TZP Sintering 02 engineering and technology Indentation hardness 03 medical and health sciences 0302 clinical medicine Wear Hardness medicine Cubic zirconia Dental enamel Ceramic Composite material Yttria-stabilized zirconia Enamel paint 030206 dentistry 020601 biomedical engineering lcsh:RK1-715 Full anatomical zirconia visual_art lcsh:Dentistry visual_art.visual_art_medium Veneer Veneered zirconia |
Zdroj: | Future Dental Journal, Vol 4, Iss 1, Pp 76-83 (2018) |
ISSN: | 2314-7180 |
Popis: | Objective The present study aimed to examine the effect of aged and polished surface treated full anatomical zirconia and veneered zirconia on wear of opposing natural human enamel surface, and investigate the surface hardness of different zirconia. Methods Two types of zirconia blocks were used in this study (Incoris ZI and Incoris TZI), Stainless Steel dies with dimensions of maxillary molars were used, duplicated using addition silicon impression material to form twenty four epoxy dies, then dies were scanned by the OmniCam. Software designing of crowns and copings was performed, then milling of the presintered blocks was done followed by separation of crowns and copings from the blocks and finishing. Sintering of zirconia blocks was done afterwards, regarding the copings feldspathic porcelain was used with the layering technique to veneer the copings to produce full anatomic crowns. All samples were then polished using special polishing kit for zirconia and glass ceramics and thermal ageing was done for two group using an autoclave at 135 °C and 2 atmospheric pressure for 5 h. The twenty-four specimens were weighed before wear testing using a sensitive electronic balance then inserted in a custom made wear machine that simulated the wear mechanism that occurs in the oral cavity with natural mandibular molars as antagonists under a weight of 5 kg (49 N) and the rotation was of 240 cycles/min, the total time of wear was 8 h, so the total cycles performed were 120,000 cycles. The twenty-four specimens were weighed again after wear testing for the weight loss measurements determination. One specimen from each tested group was randomly selected and viewed under Scanning Electron Microscope in-order to determine the wear pattern. Vicker's hardness testing was the performed for all the specimens in-order to detect Vicker's hardness number. Findings Full anatomical zirconia specimens revealed the lowest wear values when they were polished followed by higher values after thermal aging. The veneered copings showed significantly higher wear values compared to full anatomical zirconia crowns; with the aged veneered group showing the highest wear readings. These results were the same revealed with the natural enamel antagonists. As regarding hardness, full anatomical zirconia revealed better surface mechanical properties in comparison to veneered zirconia whether zirconia was polished or aged. Conclusions Yttria Stabilized Zirconia (Y-TZP) is the ceramic material of choice for all ceramic FPDs in the posterior region, since it underscored remarkable mechanical properties results, and this allowed it to be used for highly loaded ceramic restorations with high performance. |
Databáze: | OpenAIRE |
Externí odkaz: |