Using DIC techniques to measure strain ranges inside the cyclic plastic zone ahead of a fatigue crack tip
Autor: | G. L. G. Gonzáles, Jaime Tupiassú Pinho de Castro, Julián Andrés Ortiz González, José L. F. Freire |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2019 |
Předmět: |
Digital image correlation
Materials science Strain (chemistry) Mechanical Engineering lcsh:Mechanical engineering and machinery lcsh:TA630-695 lcsh:Structural engineering (General) Paris' law Measure (mathematics) Crack closure Speckle pattern Crack-tip strain field Mechanics of Materials Digital Image Correlation Damage ahead of the crack tip Stereo microscope Cyclic plastic zone lcsh:TJ1-1570 Composite material Compact tension specimen Stereo microscope measurements |
Zdroj: | Frattura ed Integrità Strutturale, Vol 13, Iss 49, Pp 74-81 (2019) Frattura ed Integrità Strutturale; Vol. 13 No. 49 (2019): July 2019; 74-81 Frattura ed Integrità Strutturale; V. 13 N. 49 (2019): July 2019; 74-81 Frattura ed Integrità Strutturale, Vol 13, Iss 49 (2019) |
ISSN: | 1971-8993 |
Popis: | A stereo microscope coupled to a 3-D Digital Image Correlation system is used to measure strain ranges on the cyclic plastic zone ahead of a fatigue crack-tip. First, a very refined speckle pattern is applied on the surface of a disk-shaped compact tension specimen of 1020 low-C steel by spraying toner powder over a layer of white paint, a suitable technique to produce the very small dots needed to map surface strain loops on that small region. This technique can achieve enough resolution to measure elastoplastic strain ranges Δε near the crack tip, which cause damage accumulation inside the cyclic plastic zone as the crack grows. The applied technique can identify as well the effects of other nonlinear phenomena that happen in the near-tip region, such as crack closure. Therefore, such measurements can be used to verify the validity of the hypotheses behind the main fatigue crack growth models. |