Improvement of rubber recipe for massive tires by addition of non-traditional fillers
Autor: | I. A. Litvinova, Y. A. Gamlitskiy, I. V. Veselov |
---|---|
Rok vydání: | 2020 |
Předmět: |
Materials science
Geography Planning and Development Recipe 02 engineering and technology TP368-456 Management Monitoring Policy and Law rubber active filler reinforcement strength fatigue characteristics 010402 general chemistry 021001 nanoscience & nanotechnology 01 natural sciences Food processing and manufacture 0104 chemical sciences Natural rubber visual_art visual_art.visual_art_medium Composite material 0210 nano-technology |
Zdroj: | Vestnik Voronežskogo Gosudarstvennogo Universiteta Inženernyh Tehnologij, Vol 81, Iss 4, Pp 196-204 (2020) |
ISSN: | 2310-1202 2226-910X |
DOI: | 10.20914/2310-1202-2019-4-196-204 |
Popis: | We investigated the effect of new fillers on the properties of rubbers for solid tires. Modified by fullerenes and unmodified iron oxide fillers were used as new fillers. Fatigue characteristics were determined by two methods: multiple tension on the UR-500 device in accordance with GOST 261-79; alternating bending with rotation on the device SZPI in accordance with GOST 10952-75. The main tasks of constructing fatigue curves were to assess the compliance of the results of strength tests (tension at a constant speed to break) with fatigue in terms of fatigue life, fatigue strength, and fatigue energy density of fracture. In addition, the task was to verify the possibility of plotting on one Weller curve points obtained on different devices - UR 500 and ZPI. The ranking of rubbers in static does not coincide with each other. Since the fatigue loading conditions are closer to the actual operating conditions than the static ones, in order to predict the behavior of rubber goods in operation, one should focus on the results of fatigue tests. Combining the results of fatigue tests with repeated tension and with alternating bending with rotation showed that this procedure is valid, but only in cases where the temperature of self-heating on the ZPI device does not exceed a certain critical value when thermal decomposition begins. The results of fatigue tests showed that the use of the studied fillers with small degrees of filling (up to 30 mass parts) can be justified. An example is Ferrocolor fraction 0–20 ?m with a mass fraction of 5 m.h. In this case, the fatigue properties practically do not deteriorate in comparison with industrial rubber for solid tires, in which new fillers are not added. |