Chemical components of shredded paper insulation: a preliminary study
Autor: | J R Millette, W F Mueller, J M Cohen, B J Kelman, L V Uppala, L J Swenson |
---|---|
Rok vydání: | 1999 |
Předmět: |
Paper
Air Pollutants Chemistry business.industry Construction Materials Public Health Environmental and Occupational Health Formaldehyde Pilot Projects Raw material Pulp and paper industry Chloride Toluene Risk Assessment Occupational Diseases chemistry.chemical_compound Indoor air quality Thermal insulation Environmental chemistry Occupational Exposure medicine Humans Cellulose insulation business medicine.drug Fire retardant |
Zdroj: | Applied occupational and environmental hygiene. 14(3) |
ISSN: | 1047-322X |
Popis: | We conducted an evaluation of shredded paper insulation to identify potentially toxic components. The study was to provide a preliminary characterization of a few samples of insulation currently in use. The following samples were analyzed: previously produced insulation (PPI) containing fire retardants, shredded recycled paper (PPI feedstock), freshly produced insulation (FPI), and insulation which had been installed in a residence (II). Volatile constituents were analyzed by GC-MS from headspace air of samples held at room temperature or heated to 90 degrees C. Extractable constituents were sampled by extracting with methylene chloride, and analyzing by GC-MS. Formaldehyde analysis was done according to EPA Method TO11. Headspace air at room temperature contained no detectable quantities of volatile constituents for any sample measured. In headspace air at 90 degrees C, only PPI contained traces of aliphatic and aromatic hydrocarbons and higher aldehydes, and FPI traces of toluene. Extracts of PPI contained traces of octadecadienoic acid methyl ester and aliphatic and aromatic hydrocarbons and higher aldehydes. Extracts of PPI feedstock contained traces of a substituted cyclohexenecarboxylic acid. FPI contained extractable diethyl phthalate (30-50 micrograms/g). Extracts of II contained traces of methyl palmitate, an octadecenoic acid methyl ester, and a phthalate plasticizer. No formaldehyde was detected. PPI was composed of approximately 98 percent paper fiber and 2 percent pre-gelatinized starch. PPI samples agglomerated together with less than 0.01 percent separating from clumps as fine dust. Boron and sodium were expected and confirmed because they were added to PPI and FPI as fire retardants. Chromium, copper, iron, potassium, magnesium, manganese, phosphorus, and silicon were present at detectable concentrations. Study calculations indicate that an occupant would have to completely consume all the fine particles produced from 3.3 kg of insulation per day to have an intake of boron equivalent to the EPA RfD. No other constituent appeared to be present even close to toxicologically relevant amounts. |
Databáze: | OpenAIRE |
Externí odkaz: |