Shear failure of AA2024 and AA7175 under high strain rate loading
Autor: | Gunasilan Manar, Patrice Longère |
---|---|
Přispěvatelé: | Institut Clément Ader (ICA), Institut Supérieur de l'Aéronautique et de l'Espace (ISAE-SUPAERO)-Institut National des Sciences Appliquées - Toulouse (INSA Toulouse), Institut National des Sciences Appliquées (INSA)-Université de Toulouse (UT)-Institut National des Sciences Appliquées (INSA)-Université de Toulouse (UT)-Université Toulouse III - Paul Sabatier (UT3), Université de Toulouse (UT)-Centre National de la Recherche Scientifique (CNRS)-IMT École nationale supérieure des Mines d'Albi-Carmaux (IMT Mines Albi), Institut Mines-Télécom [Paris] (IMT)-Institut Mines-Télécom [Paris] (IMT), Institut National des Sciences Appliquées - Toulouse (INSA Toulouse), Institut National des Sciences Appliquées (INSA)-Institut National des Sciences Appliquées (INSA)-Centre National de la Recherche Scientifique (CNRS)-Université Toulouse III - Paul Sabatier (UT3), Université Fédérale Toulouse Midi-Pyrénées-Université Fédérale Toulouse Midi-Pyrénées-IMT École nationale supérieure des Mines d'Albi-Carmaux (IMT Mines Albi), Institut Mines-Télécom [Paris] (IMT)-Institut Mines-Télécom [Paris] (IMT)-Institut Supérieur de l'Aéronautique et de l'Espace (ISAE-SUPAERO) |
Jazyk: | angličtina |
Rok vydání: | 2018 |
Předmět: |
High strain rate
Materials science Scanning electron microscope chemistry.chemical_element 02 engineering and technology Impact test 021001 nanoscience & nanotechnology High strain 020303 mechanical engineering & transports 0203 mechanical engineering chemistry Shear (geology) Aluminium lcsh:TA1-2040 [SPI.MECA.STRU]Engineering Sciences [physics]/Mechanics [physics.med-ph]/Structural mechanics [physics.class-ph] [SPI.MECA.MEMA]Engineering Sciences [physics]/Mechanics [physics.med-ph]/Mechanics of materials [physics.class-ph] Composite material 0210 nano-technology lcsh:Engineering (General). Civil engineering (General) |
Zdroj: | ICEAF V-5th International Conference of Engineering Against Failure-Proceeding ICEAF V-5th International Conference of Engineering Against Failure-Proceeding, Jun 2018, Chios Island, Greece MATEC Web of Conferences, Vol 188, p 02005 (2018) |
Popis: | In the context of the design of aeronautical structures regarding accidental events, we are here investigating and comparing the shear failure of two aluminum alloys, namely AA2024 and AA7175, under high strain rate loading. With this aim in view, two experiments were carried out: (i) high strain rate shear compression of hat shaped structures, and (ii) impact test on the edge of double notched plates. The fractured surfaces of post-mortem specimens were observed using optical and scanning electron microscopes (SEM) in order to identify the failure mechanisms. |