The Technology Transfer from Europe to China in the 17th–18th Centuries: Non-Invasive On-Site XRF and Raman Analyses of Chinese Qing Dynasty Enameled Masterpieces Made Using European Ingredients/Recipes
Autor: | Philippe Colomban, Michele Gironda, Divine Vangu, Burcu Kırmızı, Bing Zhao, Vincent Cochet |
---|---|
Přispěvatelé: | De la Molécule aux Nanos-objets : Réactivité, Interactions et Spectroscopies (MONARIS), Institut de Chimie du CNRS (INC)-Sorbonne Université (SU)-Centre National de la Recherche Scientifique (CNRS), XGLab SRL, Yildiz Technical University (YTU), Centre de recherche sur les civilisations de l'Asie Orientale (CRCAO), École pratique des hautes études (EPHE), Université Paris sciences et lettres (PSL)-Université Paris sciences et lettres (PSL)-Collège de France (CdF (institution))-Centre National de la Recherche Scientifique (CNRS)-Université de Paris (UP) |
Jazyk: | angličtina |
Rok vydání: | 2021 |
Předmět: |
China
spectroscopy Technology 02 engineering and technology 01 natural sciences Article gold alloy green [CHIM]Chemical Sciences General Materials Science Qing Dynasty cloisonné Microscopy QC120-168.85 blue 010401 analytical chemistry QH201-278.5 white 021001 nanoscience & nanotechnology Engineering (General). Civil engineering (General) yellow 0104 chemical sciences TK1-9971 painted enamels composition Descriptive and experimental mechanics Electrical engineering. Electronics. Nuclear engineering TA1-2040 0210 nano-technology |
Zdroj: | Materials; Volume 14; Issue 23; Pages: 7434 Materials, Vol 14, Iss 7434, p 7434 (2021) Materials Materials, MDPI, 2021, 14 (23), pp.7434. ⟨10.3390/ma14237434⟩ |
ISSN: | 1996-1944 |
DOI: | 10.3390/ma14237434 |
Popis: | Two masterpieces of the Qing Dynasty (1644–1912 CE), one in gilded brass (incense burner) decorated with cloisonné enamels stylistically attributed to the end of the Kangxi Emperor’s reign, the other in gold (ewer offered by Napoleon III to the Empress as a birthday present), decorated with both cloisonné and painted enamels bearing the mark of the Qianlong Emperor, were non-invasively studied by optical microscopy, Raman microspectroscopy and X-ray microfluorescence spectroscopy (point measurements and mapping) implemented on-site with mobile instruments. The elemental compositions of the metal substrates and enamels are compared. XRF point measurements and mappings support the identification of the coloring phases and elements obtained by Raman microspectroscopy. Attention was paid to the white (opacifier), blue, yellow, green, and red areas. The demonstration of arsenic-based phases (e.g., lead arsenate apatite) in the blue areas of the ewer, free of manganese, proves the use of cobalt imported from Europe. The high level of potassium confirms the use of smalt as the cobalt source. On the other hand, the significant manganese level indicates the use of Asian cobalt ores for the enamels of the incense burner. The very limited use of the lead pyrochlore pigment (European Naples yellow recipes) in the yellow and soft green cloisonné enamels of the Kangxi incense burner, as well as the use of traditional Chinese recipes for other colors (white, turquoise, dark green, red), reinforces the pioneering character of this object in technical terms at the 17th–18th century turn. The low level of lead in the cloisonné enamels of the incense burner may also be related to the use of European recipes. On the contrary, the Qianlong ewer displays all the enameling techniques imported from Europe to obtain a painted decoration of exceptional quality with the use of complex lead pyrochlore pigments, with or without addition of zinc, as well as cassiterite opacifier. |
Databáze: | OpenAIRE |