Fabrication of colloidosomes at low temperature for the encapsulation of thermally sensitive compounds
Autor: | Alexander F. Routh, Samia Laïb |
---|---|
Přispěvatelé: | Department of Chemical Engineering and BP Institute, University of Cambridge [UK] (CAM), Laïb, Samia |
Rok vydání: | 2008 |
Předmět: |
Sodium Acetate
Sintering 02 engineering and technology 01 natural sciences MESH: Plant Oils Colloid and Surface Chemistry Pulmonary surfactant Sunflower Oil chemistry.chemical_classification MESH: Sodium Acetate MESH: Surface-Active Agents Temperature MESH: Polystyrenes Polymer MESH: Sodium Hydroxide 021001 nanoscience & nanotechnology MESH: Temperature Surfaces Coatings and Films Electronic Optical and Magnetic Materials MESH: Acrylates Acrylates MESH: Colloids 0210 nano-technology Glass transition MESH: Ethanol Materials science Fabrication MESH: Microscopy Electron Scanning 010402 general chemistry Phase Transition Biomaterials Surface-Active Agents Oil phase Alkanes MESH: Water Plant Oils Sodium Hydroxide MESH: Particle Size Colloids Particle Size [SDV.IB.BIO]Life Sciences [q-bio]/Bioengineering/Biomaterials Ethanol Aqueous two-phase system Water 0104 chemical sciences [SDV.IB.BIO] Life Sciences [q-bio]/Bioengineering/Biomaterials MESH: Alkanes Chemical engineering chemistry Colloidal particle Microscopy Electron Scanning Polystyrenes MESH: Phase Transition |
Zdroj: | Journal of Colloid and Interface Science Journal of Colloid and Interface Science, Elsevier, 2008, 317 (1), pp.121-9. ⟨10.1016/j.jcis.2007.09.019⟩ |
ISSN: | 0021-9797 1095-7103 |
DOI: | 10.1016/j.jcis.2007.09.019 |
Popis: | International audience; A method using safe and mild conditions to prepare water-core colloidosomes of a few micrometers in size is examined. Using poly(styrene-co-butylacrylate) colloidal particles of 180 nm in size, with a low-temperature glass transition of 30 or 42 degrees C, the self-assembly into micrometer-sized water-core polymer shell particles is demonstrated. The effect of oil phase type, surfactant and cosolvent, sintering time, and the method of transfer into an aqueous phase are all examined. The work demonstrates the production of water-core rigid-shell colloidosomes at low temperatures, between 35 and 65 degrees C. |