Shear bond strength of glass ionomer and resin‐based cements to different types of zirconia

Autor: Matteo Buonvivere, Francesco De Angelis, Mirco Vadini, Camillo D’Arcangelo, G D Rondoni
Rok vydání: 2020
Předmět:
Zdroj: Journal of Esthetic and Restorative Dentistry. 32:806-814
ISSN: 1708-8240
1496-4155
Popis: Objective To investigate the shear bond strength (SBS) of a glass ionomer (GI) cement, an 10-methacryloyloxy-decyl dihydrogen phosphate (MDP)-based adhesive resin cement (MDP-based AC), an MDP-based self-adhesive resin cement (MDP-based SAC), an MDP-free self-adhesive resin cement (MDP-free SAC), and a resin-modified GI (RMGI) cement to a 3 mol% yttria-stabilized (3Y-TZP) and a 5 mol% yttria partially stabilized zirconia (5Y-PSZ). Materials and methods Fifty blocks were produced using 3Y-TZP and 5Y-PSZ, assigned to subgroups based on the five cements investigated (n = 10) and luted to cylindrical specimens of the same substrate. Each specimen was loaded in a SBS apparatus to failure. Mean SBS (MPa) values and standard deviations were calculated. Data were analyzed using a two-way analysis of variance and Tukey tests (α = .05). Failed specimens were subjected to fractographic analysis. Results MDP-based AC and MDP-based SAC cements displayed the highest SBS values with both the substrates; GI cement showed the lowest. RMGI and MDP-free SAC cements performed better with 3Y-TZP than with 5Y-PSZ. Fractographic analysis revealed only adhesive and mixed failures. Conclusions MDP-based AC and MDP-based SAC cements are suitable for both 3Y-TZP and 5Y-PSZ. MDP-free SAC and RMGI cements are adequate choices for 3Y-TZP, but seem less effective with 5Y-PSZ. Clinical significance MDP-based SACs appear to be as reliable as MDP-based ACs for both 3Y-TZP and 5Y-PSZ cementation. Specifically, for 5Y-PSZ cementation, resin-based MDP-free SACs do not seem to guarantee predictable results in terms of SBS.
Databáze: OpenAIRE