Journal of the Southern African Institute of Mining and Metallurgy, Volume: 122, Issue: 4, Pages: 173-180, Published: APR 2022 |
Popis: |
A sampling campaign carried out on the lead flotation circuit at Lakan lead-zinc processing plant demonstrated that the Pb recovery was only about 68-69%. Characterization of the Pb flotation tailing showed that 61.4% of the Pb is in the -37 um size fraction, which is difficult to recover by flotation. Batch flotation experiments were carried out on a plant sample of the lead flotation feed and high-intensity conditioning (HIC) was used to improve flotation recovery. The results showed that increasing the collector conditioning time from 1 to 3 minutes significantly increases the Pb recovery from 42.5% to 57.3%. Further increases in conditioning time to 5 to 7 minutes decreased the Pb recovery. With a collector conditioning time of more than 3 minutes, due to the surface cleaning effect, increasing collector and frother dosage improved the flotation selectivity and recovery, even at higher collector dosages. The Pb recovery increased from 69.1% to 79.8% with increasing impeller speed from 600 to 1250 r/min. HIC increases the flotation kinetics and greatly improves the flotation recovery and concentrate grade. |
Databáze: |
OpenAIRE |
Externí odkaz: |
|