Popis: |
In this work we study the effect of cycling in hydrogen with a purity grade 4.5 of six alloys belonging to the LaNi 5− x Sn x family for 0 ≤ x ≤ 0.5. Measurements consist in the alternate repetition of absorption reactions at a temperature of 316 K and an initial pressure of 800 kPa, each followed by a desorption reaction at the same temperature and a maximum backpressure of 2 kPa. All samples present good stability, preserving at least 98% of their initial capacity after 100 cycles. Samples with composition LaNi 5 and LaNi 4.55 Sn 0.45 were subjected to 1000 cycles, after which we observe a higher stability from the Sn-containing alloy (96% of the initial capacity preserved versus 92% for LaNi 5 ). Absorption characteristic times do not suffer important changes in either case. Desorption is gradually retarded when Sn content is higher than 0.4 at. |
Databáze: |
OpenAIRE |
Externí odkaz: |
|