La and Sm Co-doped SrTiO 3- δ Thermoelectric Ceramics
Autor: | W. Schmidt, Derek C. Sinclair, Rebecca Boston, Adindu C. Iyasara, Ian M. Reaney |
---|---|
Rok vydání: | 2017 |
Předmět: |
Materials science
Scanning electron microscope Analytical chemistry 02 engineering and technology 010402 general chemistry 021001 nanoscience & nanotechnology 01 natural sciences 0104 chemical sciences Metal Thermal conductivity Electrical resistivity and conductivity Seebeck coefficient visual_art Thermoelectric effect visual_art.visual_art_medium Relative density 0210 nano-technology Perovskite (structure) |
Zdroj: | Materials Today: Proceedings. 4:12360-12367 |
ISSN: | 2214-7853 |
DOI: | 10.1016/j.matpr.2017.10.004 |
Popis: | The thermoelectric properties of Sr1-xLax/2Smx/2TiO3-δ (0.05 ≤ x ≤ 0.30) ceramics have been investigated with compositions batched, synthesised by solid state reaction and sintered in 5% H2/N2 at 1500 °C for 6 hrs. All X-ray diffraction patterns were fully indexed according to a cubic perovskite phase. Scanning electron microscopy revealed homogeneous grain structure in the ceramics and confirmed relative density ≥ 89%. The electrical conductivity (σ) of x ≤ 0.15 displayed metallic behaviour with σ < 1000 S/cm, whereas x ≥ 0.20 were semiconducting with σ < 250 S/cm. The Seebeck coefficient of all compositions was negative indicating n-type behaviour. Within this series, x = 0.20 displayed the lowest thermal conductivity of ∼ 3 W/m.K (at 973 K), x = 0.10 displayed the highest power factor of 1400 μW/K2.m (at 573 K) and overall x = 0.15 had the highest dimensionless figure of merit (ZT) of 0.24 (at 875 K). |
Databáze: | OpenAIRE |
Externí odkaz: |