Influence of non-homogeneity of sample thickness on the determination of absolute Mössbauer fraction

Autor: T. J. Panek, M. Szuszkiewicz, J. Kansy
Rok vydání: 1983
Předmět:
Zdroj: Physica Status Solidi (a). 80:643-655
ISSN: 1521-396X
0031-8965
DOI: 10.1002/pssa.2210800229
Popis: The non-homogeneity of sample thickness and the deat-time Mossbauer effect spectrometer influences on the determining of the Debye-Waller (DW) factor are analysed. It is shown that this non-homogeneity lowers the intensity of lines and deforms the spectrum shape. To obtain the correct theoretical transmission Mossbauer spectrum it is necessary to take into consideration the electronic absorption coefficient and the term proportional to the second derivative of the transimission integral (TI) which should be added to TI. The values of DW factor at room temperature for polycrystalline sodium nitroprusside, ƒ′ = 0.367 ± 0.002, pyrite, ƒ′ = 0.855 ± 0.026, and source 57Fe in Cr, ƒ = 0.763 ± 0.005 are obtained. Der Einflus der Inhomogenitat der Probendicke und der Totzeit der Meseinrichtung auf die Debye-Waller-Faktor(DW)-Bestimmung wird analysiert. Es wird gezeigt, das die Inhomogenitat der Probendicke eine Erniedrigung der Linienintensitat und eine Spektrenverzerrung hervorruft. Das richtige theoretische Mosbauerspektrum erhalt man durch zusatzliche Berucksichtigung der elektronischen Absorption und eines Terms zum Transmissionsintegral des Mosbauerspektrums, der proportional zu der zweiten Ableitung dieses Integrals ist. Die Werte der DW-Faktoren bei Zimmertemperatur werden fur polykristallines Natriumnitroprussid, ƒ′ = 0,367 ± 0,002, fur Pyrit, ƒ′ = 0,855 ± 0,026 und fur die Quelle 57Fe in Cr, ƒ = 0,763 ± 0,005 bestimmt.
Databáze: OpenAIRE