Popis: Fatigue crack growth rates have been determined for beta-annealed Ti-6Al-4V alloys with respective oxygen contents of 0.06, 0.11, 0.18 and 0.20 wt pct. For each of these alloys, transitional crack growth behavior has been observed which appears to correlate with a critical value of the reversed plastic zone size,viz the Widmanstatten packet size. Moreover, growth rates below transitional levels order in terms of packet size, with lower growth rates associated with larger packets. The present results suggest that intersti-tial oxygen content and prior beta grain size significantly affect fatigue crack growth rates through control of the Widmanstatten packet size.