Sustainability and the Environment Chemistry Open-circuit voltage Membrane electrode assembly Analytical chemistry Condensed Matter Physics Cathode Surfaces Coatings and Films Electronic Optical and Magnetic Materials Anode law.invention chemistry.chemical_compound Membrane Transmission electron microscopy law Electrode Materials Chemistry Electrochemistry Fluoride |
Zdroj: | Journal of The Electrochemical Society. 154:B757 |
ISSN: | 0013-4651 |
DOI: | 10.1149/1.2741129 |
Popis: | The correlation between the degradation behavior of a membrane electrode assembly (MEA) and deposited Pt (Pt band) in the membrane during an open-circuit voltage hold test was studied. The degradation behavior was investigated by measuring the fluoride ion emission in the effluent water from the anode and the cathode for various gas compositions at both electrodes. The results showed that the fluoride ion emission rate (PER) varied in accordance with the gas compositions. Cross sections of the tested MEAs were observed using a transmission electron microscope. It was found that the location of the Pt band correlated with the magnitude of the FERs. The Pt band was located close to where the mixed potential in the membrane, which was determined by the gas compositions, changed dramatically. |
Databáze: | OpenAIRE |
Externí odkaz: |