FeAl–TiN nanocomposite produced by reactive ball milling and hot-pressing consolidation
Autor: | M. Krasnowski, T. Kulik |
---|---|
Rok vydání: | 2003 |
Předmět: | |
Zdroj: | Scripta Materialia. 48:1489-1494 |
ISSN: | 1359-6462 |
DOI: | 10.1016/s1359-6462(03)00112-x |
Popis: | The FeAl–TiN nanocomposite was produced by milling an elemental powder mixture of Al–Fe–Ti in nitrogen, followed by hot-pressing consolidation under 8 GPa of pressure. The average hardness of the nanocomposites consolidated at temperatures of 750 and 950 °C are 1424 HV 0.2 and 1461 HV 0.2 respectively, and the density is 97% of the theoretical value in both cases. |
Databáze: | OpenAIRE |
Externí odkaz: |