Strength of welded joint sunder quasi -brittle fracture

Autor: M. V. Shakhmatov, E. A. Usmanova
Rok vydání: 2020
Předmět:
Zdroj: Journal of Physics: Conference Series. 1441:012114
ISSN: 1742-6596
1742-6588
DOI: 10.1088/1742-6596/1441/1/012114
Popis: In the study of the crack resistance of welded joints with constructive incomplete welds, which are regulated by welding GOSTs and have a wide practice of application, including for critical structures, it is necessary to keep in mind that these stress concentrators on the sharpness of their tops are significantly different from fatigue and operational cracks. Welding defects have the same difference: faulty welds, faulty fusions, undercuts. This paper shows that the strength of welded joints with structural faulty welds in addition to mechanical characteristics and the length of the faulty weld also depends on the radius at its top. Based on the ratios of fracture mechanics, a strain fracture criterion is proposed -the critical opening of the concentrator under consideration, depending on the radius at its top. At the same time, with the reduction of the radius at the top of the concentrator to a certain critical value, comparable to the radius at the top of the crack, the proposed criterion coincides with the material characteristic according to GOST 25.506-85 – the critical crack opening. Dependence for assessing the quasi-brittle strength of welded joints with faulty welds based on the critical disclosure of the concentrator under consideration satisfactorily corresponds to the experimental data on samples from the AMg6 alloy.
Databáze: OpenAIRE