Popis: | LaFe11.6Si1.4 alloys have been successfully fabricated by spark plasma sintering (SPS). An annealing study of the SPS LaFe11.6Si1.4 alloys at different temperatures ranging from 1373 to 1523 K for annealing times from 30 minutes to 72 hours was carried out. This annealing study showed that LaFe11.6Si1.4 samples annealed at 1473K (for annealing times between 30 minutes and 6 hours) have a significantly higher amount of the NaZn13-type phase compared to samples annealed at other temperatures. Thus the critical annealing temperature which enhances the formation of the NaZn13-type phase in SPS LaFe11.6Si1.4 compounds is 1473K. A second study investigated the effect of different particle sizes of the starting powders on the formation of the NaZn13-type phase. This study found that the samples synthesized using larger sized powder particles exhibited a significantly higher amount of the NaZn13-type phase compared to samples synthesized using smaller sized powder particles, for the same heat treatment. |
Databáze: | OpenAIRE |
Externí odkaz: |