Design of binder jet additive manufactured co-continuous ceramic-reinforced metal matrix composites
Autor: | Norman Y. Zhou, Yahya Mahmoodkhani, Hashem Al Momani, Ehsan Marzbanrad, Pablo D. Enrique, Ehsan Toyserkani, Ali Keshavarzkermani |
---|---|
Rok vydání: | 2020 |
Předmět: |
Materials science
Polymers and Plastics Alloy Sintering 02 engineering and technology engineering.material 010402 general chemistry 01 natural sciences Carbide Whisker Materials Chemistry Ceramic Composite material Mechanical Engineering Metal matrix composite Metals and Alloys 021001 nanoscience & nanotechnology 0104 chemical sciences Superalloy Mechanics of Materials visual_art Volume fraction Ceramics and Composites engineering visual_art.visual_art_medium 0210 nano-technology |
Zdroj: | Journal of Materials Science & Technology. 49:81-90 |
ISSN: | 1005-0302 |
DOI: | 10.1016/j.jmst.2020.01.053 |
Popis: | Ceramic-reinforced metal matrix composites (MMCs) display beneficial properties owing to their combination of ceramic and metal phases. However, the properties are highly dependent on the reinforcing phase composition, volume fraction and morphology. Continuous fiber or network reinforcement morphologies are difficult and expensive to manufacture, and the often-used discontinuous particle or whisker reinforcement morphologies result in less effective properties. Here, we demonstrate the formation of a co-continuous ceramic-reinforced metal matrix composite using solid-state processing. Binder jet additive manufacturing (BJAM) was used to print a nickel superalloy part followed by post-processing via reactive sintering to form a continuous carbide reinforcing phase at the particle boundaries. The kinetics of reinforcement formation are investigated in order to develop a relationship between reactive sintering time, temperature and powder composition on the reinforcing phase thickness and volume fraction. To evaluate performance, the wear resistance of the reinforced BJAM alloy 625 MMC was compared to unreinforced BJAM alloy 625, demonstrating a 64 % decrease in the specific wear rate under abrasive wear conditions. |