Comparsion of the shear bond strength of ceramic brackets bonded to porcelain fused metal crowns and metal free ceramic crowns with and without silane coupling agent- an in vitro study
Autor: | Kuldeep Dmello, Rahul Pawar, Shreya Sharma, Dip Gautam Choudhary, Bhupendra Singh |
---|---|
Rok vydání: | 2020 |
Předmět: |
Primer (paint)
Materials science Bond strength Silane coupling 030206 dentistry engineering.material Metal 03 medical and health sciences 0302 clinical medicine Metal free visual_art visual_art.visual_art_medium engineering Cubic zirconia 030212 general & internal medicine Ceramic Composite material Buffered oxide etch |
Zdroj: | IP Indian Journal of Orthodontics and Dentofacial Research. 6:236-240 |
ISSN: | 2581-9364 2581-9356 |
DOI: | 10.18231/j.ijodr.2020.046 |
Popis: | Aim: The aim of this study is to evaluate and compare the shear bond strength of ceramic brackets bonded to porcelain fused metal crowns and metal free ceramic crowns with and without silane coupling agent. Materials and Methods: 40 metal free zirconia crowns and 40 PFM crowns were fabricated with glazed surfaces according to the manufacturer’s instructions for the study purpose. The samples were divided in two groups A and B and each group was subdivided into two subgroups (A1, A2) and (B1, B2) Sub-Group A1 and A2: Twenty metal free ceramic crowns were etched with 9% buffered HF acid gel for 2 minutes, thoroughly washed and air dried. Relyx ceramic primer (silane coupling agent) was applied to the treated surface. Subgroup B1 and B2: 20 porcelain fused metal crowns were etched with 9% buffered HF acid gel for 2 minutes, thoroughly washed and air dried. Relyx ceramic primer (silane coupling agent) was applied to the treated surface. The shear bond strength of ceramic brackets bonded to porcelain fused metal crowns and metal free ceramic crowns with and without silane coupling agent. Statistical Analysis: ANOVA and Post hoc Tukey’s test (HSD) tests were used for statistical analysis. Result: The result showed that group B1 demonstrate the maximum shear bond strength among all groups which is 9%HF +Relyx ceramic primer application on porcelain fused metal crowns (10.27+1.31Mpa) and has highly significant value. Whereas lowest shear bond strength belongs to group B2which is 9%HF and primer is not applied (5.4+0.73 MPa). Conclusion: Hence it can be concluded that Relyx ceramic primer is more aooropriate choice for bonding orthodontic metal brackets on PFM and zirconia surfaces with conventional bonding system. Keywords: Porcelain fused metal, Shear bond strength, Ceramic brackets, Megapascals. |