Phase composition and properties of austenitic-ferritic 0Kh21N6M2T steel
Autor: | A. P. Okenko, A. D. Devchenko, M. N. Kul'kova |
---|---|
Rok vydání: | 1967 |
Předmět: | |
Zdroj: | Metal Science and Heat Treatment. 9:320-322 |
ISSN: | 1573-8973 0026-0673 |
DOI: | 10.1007/bf00652978 |
Popis: | 1. High-temperature tests of steel as cast and hot-rolled showed high ductility at 900–1200°C, which ensures high plasticity in hot working. 2. Tempering 1 h at 400–900°C does not lead to embrittlement of samples quenched from 1200–1020°C. The samples are embrittled by prolonged tempering (10 and 100 h) at 600–800°C. 3. Embrittlement is due to the precipitation of the σ-phase at the ferrite-austenite interface. 4. The brittleness is removed by heating 1 h at temperatures above 900°C, which dissolves the σ-phase. |