Autor: |
N. Otake, A. Yoshikawa, Manabu Satou, Akira Hasegawa, Shuhei Nogami, Yutai Katoh, Kenji Okuno, Yasuhisa Oya |
Rok vydání: |
2008 |
Předmět: |
|
Zdroj: |
Fusion Engineering and Design. 83:1490-1494 |
ISSN: |
0920-3796 |
DOI: |
10.1016/j.fusengdes.2008.06.004 |
Popis: |
In order to evaluate the oxidation behavior and mechanism of SiC/SiC composites with conventional pyrolitic graphite interface (PyC-SiC/SiC) and advanced multilayer interface (ML-SiC/SiC) in a HCSB blanket environment, a thermal gravimetric analysis (TGA) in He + O2 environment at 1000 °C and 1200 °C was performed. The PyC-SiC/SiC at 1200 °C and the ML-SiC/SiC at 1000 °C and 1200 °C showed relatively smaller weight change during oxidation because SiO2 formed on the SiC-matrix and SiC-fiber sealed the specimen surface before the PyC interface recession by gasification of graphite due to relatively high SiO2 formation rate. While the PyC-SiC/SiC at 1000 °C showed significant weight loss because the specimen surface was not sealed by SiO2 and significant PyC interface recession occurred due to relatively slow SiO2 formation. |
Databáze: |
OpenAIRE |
Externí odkaz: |
|