Popis: This paper analyzed the morphology and reasons of pitting corrosion perforation of 0Cr18Ni9 stainless steel cooling water pipes in a power plant and pointed out the measures to prevent the pitting corrosion under this condition. The results showed that: the reason of pitting corrosion of 0Cr18Ni9 stainless steel cooling water pipes was the existence of multiple Cl-and easily fouling Ca2+ and Mg2+ in water, with the corrosion products mainly the oxides of Fe and Cr; the economic measures to prevent pitting corrosion were to increase the pH of water and decrease the content of Ca2+ and Mg2+.