Occurrence of brittleness in thick-sheet 1Kh21N5T steel

Autor: M. N. Kul'kova, N. I. Ignatova
Rok vydání: 1965
Předmět:
Zdroj: Metal Science and Heat Treatment. 7:194-197
ISSN: 1573-8973
0026-0673
DOI: 10.1007/bf00658534
Popis: 1. To eliminate brittleness in 1Kh21N5T steel, the heating temperature prior to rolling should be 1100–1130°C, the optimum quenching temperature 1020°C, and the alkalization temperature not above 360°C. 2. To improve the plastic properties and reduce susceptibility to embrittlement the titanium content should be 0.25–0.50% Ti.