Comparison of the properties and catalytic activity of commercially and laboratory prepared Mg/Al mixed oxides in aldol condensation of cyclohexanone with furfural
Autor: | Zdeněk Tišler, Uliana Akhmetzyanova, Lenka Pelíšková, Romana Velvarská, David Kadlec |
---|---|
Rok vydání: | 2018 |
Předmět: |
Hydrotalcite
010405 organic chemistry Brucite Cyclohexanone engineering.material 010402 general chemistry Furfural 01 natural sciences Catalysis 0104 chemical sciences law.invention chemistry.chemical_compound chemistry law Acetone engineering Calcination Aldol condensation Physical and Theoretical Chemistry Nuclear chemistry |
Zdroj: | Reaction Kinetics, Mechanisms and Catalysis. 126:219-235 |
ISSN: | 1878-5204 1878-5190 |
DOI: | 10.1007/s11144-018-1497-7 |
Popis: | In recent years, for deeper understanding of the behavior of various heterogeneous catalysts, aldol condensation of acetone and furfural has been researched in detail. In this article, the carbonyl reactants are represented by cyclohexanone and furfural as the platform chemicals for synthesis the fundamental building blocks for future biorefineries. Our main goal was to explore the structural and acid–base properties and to compare them with catalytic characteristics of Mg/Al mixed oxides in aldol condensation of cyclohexanone with furfural. The aforesaid basic heterogeneous catalysts were obtained by the calcination of commercially and laboratory prepared hydrotalcites with different molar ratios (1:1–5:1). Their physicochemical properties were determined based on several analytical methods: XRD, ICP-OES, SEM, N2 physisorption, TGA, TGA-MS, DRIFT, TPD-CO2 and TPD-NH3. Through XRD, it was found that as-synthesized laboratory hydrotalcites had the pure crystalline hydrotalcite structure while commercial ones contained also the brucite and MgO phases. By using TPD-CO2 and TPD-NH3, the measured values, especially the total amount of basic sites, provided the best correlation with the catalytic activity of investigated catalysts. Comparable conversions of furfural (ca. 87%) were achieved on laboratory and commercial mixed oxides with the Mg/Al molar ratio 1:1 and 3:1, respectively. They had no obvious difference in selectivity to FCH (about 20%) whereas the commercial samples showed higher selectivity to F2CH (26% at max conversion) than the laboratory ones (17%). |
Databáze: | OpenAIRE |
Externí odkaz: |