Autoclave cladding of aluminum and tungsten carbide powders with nickel
Autor: | G. F. Rezvanov, I. N. Gorbatov, R. Sh. Kanashvili, I. M. Kartvelishvili, A. E. Terent'ev, N. S. Il'chenko |
---|---|
Rok vydání: | 1990 |
Předmět: |
Cladding (metalworking)
Materials science Metallurgy Metals and Alloys chemistry.chemical_element Nickel deposition Condensed Matter Physics Carbide chemistry.chemical_compound Nickel chemistry Mechanics of Materials Aluminium Tungsten carbide Metallic materials Materials Chemistry Ceramics and Composites |
Zdroj: | Soviet Powder Metallurgy and Metal Ceramics. 29:433-435 |
ISSN: | 1573-9066 0038-5735 |
DOI: | 10.1007/bf00795336 |
Popis: | tors: ensuring effective mixing and preventing nickel deposition on the current terminal. It was also important to bear in mind that introducing 75-80% nickel into the powder increased the latter's weight fourto fivefold. With small charges (30-40 g/dm=), a considerable proportion of the nickel was deposited on the current terminal. Increasing the charge to 100-120 g/dm 2 improved the quality of mixing of the powder. The optimum charge was 70 • 1 g/dm 2 when 75-80 wt.% Ni was introduced into the powder. |
Databáze: | OpenAIRE |
Externí odkaz: |