Three electrodeposited Ni–18 wt.% Fe samples were annealed at 400 °C for 3 h (hrs), 8 h, and 24 h to study the effects of grain size on the electrochemical properties of bulk Ni–18 wt.% Fe in 3.5 wt.% NaCl. The electrochemical results from the annealed samples are compared with those measured for the as-received Ni–18 wt.% Fe material consisting of an average grain size of 23 nanometers (nm). Of the four materials studied, the as-received nanocrystalline alloy less sensitive to localized corrosion. |