Utilization of partially liquefied bark for production of particleboards
Autor: | Wen Jiang, Stergios Adamopoulos, Reza Hosseinpourpia, Jure Žigon, Marko Petrič, Milan Šernek, Sergej Medved |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2022 |
Předmět: |
bark
partial liquefaction wood-based panels lcsh:Technology bonding debelinski nabrek lcsh:Chemistry skorja Wood Science udc:630*8 lcsh:QH301-705.5 lepljenje lcsh:T absorpcija vode MUF adhesives leseni ploščni kompoziti water vapor sorption thickness swelling lcsh:QC1-999 lcsh:Biology (General) lcsh:QD1-999 lcsh:TA1-2040 MUF lepilo Trävetenskap delno utekočinjen les lcsh:Engineering (General). Civil engineering (General) lcsh:Physics |
Zdroj: | Applied sciences, vol. 10, no. 15, 5253, 2020. Applied Sciences Volume 10 Issue 15 Applied Sciences, Vol 10, Iss 5253, p 5253 (2020) |
ISSN: | 2076-3417 |
Popis: | Bark as a sawmilling residue can be used for producing value-added chemicals and materials. This study investigated the use of partially liquefied bark (PLB) for producing particleboard with or without synthetic adhesives. Maritime pine (Pinus pinaster Ait.) bark was partially liquefied in the presence of ethylene glycol and sulfuric acid. Four types of particleboard panels were prepared with a PLB content of 4.7%, 9.1%, 20%, and 33.3%, respectively. Another five types of particleboard panels were manufactured by using similar amounts of PLB and 10 wt.% of melamine&ndash urea&ndash formaldehyde (MUF) adhesives. Characterization of bark and solid residues of PLB was performed by Fourier transform infrared spectroscopy (FTIR), thermogravimetric analysis (TGA), and automated vapor sorption (AVS). Mechanical and physical properties of the particleboard were tested according to the European standards EN 310 for determining modulus of elasticity and bending strength, EN 317 for determining thickness swelling after immersion in water, and EN 319 for determining internal bond strength. The results showed that the increase in PLB content improved the mechanical strength for the non-MUF boards, and the MUF-bonded boards with up to 20% of PLB met the requirements for interior uses in dry conditions according to EN 312. The non-MUF boards containing 33.3% of PLB and the MUF-bonded boards showed comparable thickness swelling and water absorption levels compared to the reference board. |