Analiza parametra translucencije staklokeramike izrađene različitim tehnološkim postupcima
Autor: | Karla Ledić, Igor Majnarić, Slađana MILARDOVIĆ ORTOLAN, Stjepan Špalj, Sanja Štefančić, Ketij Mehulić |
---|---|
Jazyk: | angličtina |
Rok vydání: | 2015 |
Předmět: | |
Zdroj: | Acta stomatologica Croatica : International journal of oral sciences and dental medicine Volume 49 Issue 1 Acta Stomatologica Croatica, Vol 49, Iss 1, Pp 27-35 (2015) |
ISSN: | 1846-0410 0001-7019 |
Popis: | Svrha: Analizirati parametar translucencije (TP vrijednosti) staklokeramika izrađenih različitim tehnološkim postupcima te ispitati kako na TP vrijednosti utječu korozivna sredstva. Materijali i metode: Izrađena su po tri uzorka IPS e.max keramike (Ivoclar Vivadent, Schaan, Lihtenštajn) u trima bojama (A2, C2 i B3) s trima različitim tehnologijama izrade (slojevanje – e.max Ceram Dentin; toplo-tlačna tehnika – e.max Press; strojno – e.max CAD). Uzorci su bili u obliku pločica dimenzija 10 mm x 12 mm x 0,8 mm. Spektrofotometrom (X-Rite DTP 20 Pulse, Neu Isenburg, Njemačka) izmjerene su CIE L*a*b* vrijednosti za izračun parametra tanslucencije (TP vrijednost) prije i poslije izlaganja 4-postotnoj octenoj kiselini na 80 °C tijekom 16 sati (ISO 6872). Statistički podatci obrađeni su programom IBM SPSS 22. Rezultati: Značajno najmanje TP vrijednosti imao je IPS e.max Ceram Dentin, a najveće IPS e.max Press u svim bojama, prije i poslije izlaganja kiselini (p The purpose of the study was to analyse translucency parameter (TP values) of glass-ceramics fabricated by different techniques and investigate the effect of the corrosive medium on TP values. Materials and methods: Three specimens of each type of IPS e.max ceramics (Ivoclar Vivadent, Schaan, Liechtenstein) were made in three colours (A2, C2 and B3) by three fabrication techniques (layering – e.max Ceram Dentin; heat-pressing – e.max Press; CAD/CAM – e.max CAD). Specimens were made in the form of plates (10 mm x 12 mm x 0.8 mm). CIE L*a*b* values were measured by a spectrophotometer (X-Rite DTP 20 Pulse, Neu Isenburg, Germany) before and after exposure to 4% acetic acid at 80 °C for 16 hours (ISO 6872) to calculate translucency parameter (TP values). Statistical data were analysed using the IBM SPSS 22 software. Results: IPS e.max Ceram Dentin had significantly the lowest TP values, and IPS e.max Press the highest TP values of all colours (A2, C2, B3), both prior and after exposure to acid (p |
Databáze: | OpenAIRE |