Sintering behavior of 45S5 bioactive glass
Autor: | Lefebvre, Leila, Gremillard, Laurent, Chevalier, Jérome, Zenati, Rachid, Bernache-Assollant, Didier |
---|---|
Přispěvatelé: | Matériaux, ingénierie et science [Villeurbanne] (MATEIS), Université Claude Bernard Lyon 1 (UCBL), Université de Lyon-Université de Lyon-Institut National des Sciences Appliquées de Lyon (INSA Lyon), Institut National des Sciences Appliquées (INSA)-Université de Lyon-Institut National des Sciences Appliquées (INSA)-Centre National de la Recherche Scientifique (CNRS), Noraker (Noraker-V), Noraker, Centre Ingénierie et Santé (CIS-ENSMSE), École des Mines de Saint-Étienne (Mines Saint-Étienne MSE), Institut Mines-Télécom [Paris] (IMT)-Institut Mines-Télécom [Paris] (IMT), Département Biomécanique et Biomatériaux (DB2M-ENSMSE), Institut Mines-Télécom [Paris] (IMT)-Institut Mines-Télécom [Paris] (IMT)-CIS, Laboratoire des Procédés en Milieux Granulaires (LPMG-EMSE), Institut Mines-Télécom [Paris] (IMT)-Institut Mines-Télécom [Paris] (IMT)-Centre National de la Recherche Scientifique (CNRS), Institut Fédératif de Recherche en Sciences et Ingénierie de la Santé (IFRESIS-ENSMSE), Institut Mines-Télécom [Paris] (IMT)-Institut Mines-Télécom [Paris] (IMT)-IFR143, INSA Lyon |
Jazyk: | angličtina |
Rok vydání: | 2008 |
Předmět: | |
Zdroj: | Acta Biomaterialia Acta Biomaterialia, Elsevier, 2008, 4 (6), pp.1894-1903 |
ISSN: | 1742-7061 |
Popis: | In this study, we report on the effect of Bioglass (R) structural transformations on its sintering behaviour. While heating up to 1000 degrees C, five successive transformations occur: glass transition, glass-in-glass phase separation, two crystallization processes and a second glass transition. The sintering of the material exhibits two main shrinkage stages associated with the two glass transitions at 550 and 850 C. At 580 degrees C, the glass-in-glass phase separation induces a decrease in the sintering rate immediately followed by the major crystalline phase crystallization (Na2CaSi2O6) between 600 and 700 degrees C, from the surface to the bulk of the particles. A complete inhibition of sintering takes place followed by a minor shrinkage effect due to crystallization. A plateau is then observed until the second glass transition temperature is reached. A modification of Frenkel's model allows the determination of the glass-in-glass phase separation kinetics and the identification of the structural transformations effects on sintering behaviour. |
Databáze: | OpenAIRE |
Externí odkaz: |