Autor: |
Ucbeyiay, Havvanur, Eker, Y. Ramazan, Ozkan, Emine |
Zdroj: |
Canadian Metallurgical Quarterly; July 2024, Vol. 63 Issue: 3 p699-711, 13p |
Abstrakt: |
ABSTRACTThis study was carried out to investigate the production of manganese nanomaterials by enriching fine-grained and low-grade manganese ores. Ore was taken from Balıkesir region in Turkey. Experimental studies were discussed in two different stages. In the first stage, the ore was enriched by a leaching method and optimum enrichment conditions were determined. For this, different mixtures of acids and reducing agents were used. The optimum Mn dissolution was 120 minutes. 97.05% Mn dissolution efficiency was obtained from the ore containing 29% MnO under a 120 minute leaching time, 600 rpm stirring speed, 2 M HCl and HNO3 (3:1) concentration, 0.5 M citric acid + 10% molasses reducers and at 90 °C. In the second stage, the Mn solution dissolved under optimum conditions was photo-reduced by exposure to sunlight and then MnCO3 was produced using Na2CO3. The produced MnCO3 was roasted and 200 nm MnO2 nanorods were obtained. |
Databáze: |
Supplemental Index |
Externí odkaz: |
|