Wear Resistance of Pre-ECAP Annealing A356 Al Alloy with 1.5 Wt.% TiB2

Autor: Syukron, Muhammad, Hussein, Zuhailawati, Anasyida, Abu Seman
Zdroj: Materials Science Forum; July 2019, Vol. 961 Issue: 1 p118-125, 8p
Abstrakt: The combination of heat treatment, addition of grain refiner and ECAP processing is used to improve mechanical properties and wear resistance of A356 Al alloys with 1.5 wt.% TiB2. The alloys were grouped into as-cast and pre-ECAP annealing. The alloys were characterized with hardness and wear testing, optical microscopy and SEM. The ECAP processing was done through BA route for 4 passes and it improved hardness, distribution of TiB2 and Si particles in the aluminium matrix and increased wear resitance of pre-ECAP annealing specimen.