Influence of Degrease Rate of Larix by High Temperature and Pressure

Autor: Qi, Hua Chun, Sun, Yao Xing
Zdroj: Applied Mechanics and Materials; February 2014, Vol. 513 Issue: 1 p147-150, 4p
Abstrakt: Northeast of Larix was degreased by high temperature and pressure steam-vacuum, and study the best conditions of degreasing, different thickness and moisture content of specimens at temperature, time, and vacuum degreasing and drying, testing its degrease rate . The results showed that the degrease rate of wood treated with high temperature and pressure steam-vacuum treatment was significantly improved. The study dealing with conditions can make degrease rate of larch 63.05%.