Infrared dichroism and birefringence studies of silica-filled styrene–butadiene rubbers

Autor: Bokobza, L., Ladouce, L., Bomal, Y., Amram, B.
Zdroj: Journal of Applied Polymer Science; 24 October 2001, Vol. 82 Issue: 4 p1006-1012, 7p
Abstrakt: Infrared and birefringence measurements are used to characterize the orientational behavior of silica-filled styrene–butadiene copolymers. The orientational data are correlated with the results of equilibrium swelling measurements. On the other hand, the role played by a silane couling agent bis(3-triethoxysilylpropyl)tetrasulfide (TESPT), or “Si69”) on rubber/silica system is discussed. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 82: 1006–1012;2001