Autor: |
Kotkis, M. A., Nabutovskii, L. Sh., Ostrov, A. E., Zil'berman, A. G. |
Zdroj: |
Metal Science and Heat Treatment; October 1985, Vol. 27 Issue: 10 p753-755, 3p |
Abstrakt: |
1.Spheroidal inclusions from 20 to 200 µm in size causing a decrease in the specific work for failure are observed in KhN77TYuR-VD alloy.2.The inclusions observed have a lamellar structure. The outer layer with a developed surface (walnut type) consists of phases containing silicon, sulfur, and magnesium while the inner core (or lamellar spheroid) contains titanium (titanium carbide), chromium, iron, and nickel. |