1.The presence of >103 per cm2 of fracture surface of large colonies consisting of lamellar inclusions and a large number of fine lamellar inclusions in the boundaries of crystals lowers the plasticity and facilitates the development of high-temperature brittleness of alloys KhN75MBTYu and KhN78T.2.Preliminary heating of alloy KhN75MBTYu with low plasticity at 750–1000° for 1–20 h does not remove high-temperature brittleness.3.Heating at temperatures above 1000° leads to partial solution and coalescence of pellicular inclusions, resulting in an increase of the fracture toughness at room temperature. |