Resistance of maraging steel N18K9M5T to cyclic impact loads

Autor: Maloletnev, A. Ya., L'vov, Yu. B., Pestov, I. V., Perkas, M. D.
Zdroj: Metal Science and Heat Treatment; July 1975, Vol. 17 Issue: 7 p584-588, 5p
Abstrakt: 1.Heat 2 has a higher resistance to cyclic impact loading and crack propagation than heats 1, 3, and 4.2.The optimal heat treatment for heat 2 to obtain the best resistance to cyclic impact loading with acting stress s=180 kg/mm2 is aging at 490° for 3 h, and aging at 510° for 3 h at lower stresses.3.Surface hardening (shotpeening) increases the resistance to impact loading more substantially for heat 1 than heat 3.