Conclusions 1.Adding a small amount of rhenium to TsM10 alloys based on molybdenum leads to an increase in strength and ductility characteristics in the temperature range 293–2073°K.2.With all of the temperatures considered (1473, 2273, and particularly 1773 and 1973°K) Mo-Re alloy has higher creep and stress-rupture strength characteristics compared with alloy TsM10. With an increase in test duration the difference between the stress-rupture strength characteristics for the test alloys at test temperatures of 1773 and 1973, and particularly 2273°K decreases. |